Icon23 Aero-Engines


Aero-Engines

Hotter, Stiffer, Stronger, Lighter Where does the aero-engine go next?



Download this document in B&W printable form (PDF format).




The pas
t shows the future will be hotter

The figure on the left shows that the remarkable improvements in aero-engine performance have come about because the materials designer has been able to provide the engineer with materials can be used at hotter temperatures. Higher engine temperatures are needed so that the engines can run more efficiently, while weight reductions require stiffer, stronger, and lighter materials.
If you can't stand the heat!

The hot parts of the engine require materials which can operate at 1000C, the cooler parts at 600C. Furthermore, the environment is very harsh chemically and mechanically, with very large forces generated by the high rotational speeds and even the possibility of birds being sucked into the engine! The maximum service temperature chart (on the right) is a useful way of identifying new possibilities for materials development.
By drawing lines at 600C and 1000C it is possible to identify the materials classes which might be suitable in this case, namely metals and ceramics. At the present time titanium and nickel alloys are used for the low and high temperature parts.
Why not ceramics?




To see why ceramics, which appear to have the best high temperature properties, are not used in aero-engines it is helpful to consider other properties which are important.
Property
Metals
Ceramics

Toughness (bird strikes)GoodVery PoorOxidation/corrosion resistanceFairGoodFormingGood (forging)Fair (sintering)JoiningGoodDifficultCreep resistanceFairGoodCostHighHigh
Poor toughness is the main reason why ceramics have not been successfully introduced into the majority of engines, but research continues.



The tricks Materials Scientists play

Materials scientists have worked hard to increase the operating temperature of today's alloys:
  • turbine blades are 'grown' as single crystals, because these are more resistant to creep (gradual changes in dimensions under stress and temperature);
  • current nickel superalloys contain expensive alloying elements such as Hafnium and Rhenium in order to increase their high temperature performance;
  • turbine blades have little networks of holes to air-cool the blade surface.


Ceramic coatings - the way ahead?



While ceramics cannot yet be used for major components, Zirconia (ZrO) coatings are being used to increase the operating temperatures. These coatings can operate at much higher temperatures and protect the metal from chemical attack.
Oxides (e.g. ZrO, Al2O3) are often used for high temperature coatings. Combined, the effects of air cooling and ceramic coatings mean that the combusting gases can reach temperatures over 1600C - higher than any metal can work.

Sponsored Links

()



« | »



Chinook Engine 1 26-05-2011 11:16 AM
Model Jet Engines wise_55 1 20-01-2011 05:22 PM
( ) General Mechanical 3 27-07-2010 07:38 PM
Galleries and new techniques 3 04-07-2010 05:56 PM
0 02-08-2009 08:04 AM


03:10 PM.

..

RSS RSS 2.0 XML XML2 SiteMap SiteMap2 ARCHIVE HTML HTML2 EXTERNAL JS URLLIST

- -     

Powered by vBulletin® Version 3.8.4, Copyright ©2000 - 2014, Jelsoft Enterprises Ltd. TranZ By Almuhajir